Recent advances in the development of GTR/GBR membranes for periodontal regeneration—A materials perspective
MC Bottino, V Thomas, G Schmidt, YK Vohra, TMG Chu, MJ Kowolik, ...
Dental materials 28 (7), 703-721, 2012
24062012
Parametric studies on self-repairing approaches for resin infused composites subjected to low velocity impact
M Motuku, UK Vaidya, GM Janowski
Smart Materials and Structures 8 (5), 623, 1999
3311999
A novel spatially designed and functionally graded electrospun membrane for periodontal regeneration
MC Bottino, V Thomas, GM Janowski
Acta biomaterialia 7 (1), 216-224, 2011
3032011
Morphology and mechanical properties of Nylon 6/MWNT nanofibers
MV Jose, BW Steinert, V Thomas, DR Dean, MA Abdalla, G Price, ...
Polymer 48 (4), 1096-1104, 2007
2152007
Thermoplastic sandwich structure design and manufacturing for the body panel of mass transit vehicle
H Ning, GM Janowski, UK Vaidya, G Husman
Composite structures 80 (1), 82-91, 2007
2122007
Influence of low‐temperature environmental exposure on the mechanical properties and structural stability of dental zirconia
TF Alghazzawi, J Lemons, PR Liu, ME Essig, AA Bartolucci, GM Janowski
Journal of Prosthodontics: Implant, Esthetic and Reconstructive Dentistry 21 …, 2012
1562012
Effects of moisture and UV exposure on liquid molded carbon fabric reinforced nylon 6 composite laminates
S Pillay, UK Vaidya, GM Janowski
Composites Science and Technology 69 (6), 839-846, 2009
1472009
Effect of grain size on the monoclinic transformation, hardness, roughness, and modulus of aged partially stabilized zirconia
TJ Lucas, NC Lawson, GM Janowski, JO Burgess
Dental Materials 31 (12), 1487-1492, 2015
1402015
The failure load of CAD/CAM generated zirconia and glass-ceramic laminate veneers with different preparation designs
TF Alghazzawi, J Lemons, PR Liu, ME Essig, GM Janowski
The Journal of prosthetic dentistry 108 (6), 386-393, 2012
1142012
Design, manufacture and analysis of a thermoplastic composite frame structure for mass transit
H Ning, U Vaidya, GM Janowski, G Husman
Composite Structures 80 (1), 105-116, 2007
1082007
Liquid molding of carbon fabric-reinforced nylon matrix composite laminates
S Pillay, UK Vaidya, GM Janowski
Journal of Thermoplastic Composite Materials 18 (6), 509-527, 2005
1042005
Effect of environmental weathering on flexural creep behavior of long fiber-reinforced thermoplastic composites
VS Chevali, DR Dean, GM Janowski
Polymer Degradation and Stability 95 (12), 2628-2640, 2010
842010
Evaluation of the optical properties of CAD-CAM generated yttria-stabilized zirconia and glass-ceramic laminate veneers
TF Alghazzawi, J Lemons, PR Liu, ME Essig, GM Janowski
The Journal of prosthetic dentistry 107 (5), 300-308, 2012
832012
Flexural creep behavior of discontinuous thermoplastic composites: Non-linear viscoelastic modeling and time–temperature–stress superposition
VS Chevali, DR Dean, GM Janowski
Composites Part A: Applied Science and Manufacturing 40 (6-7), 870-877, 2009
822009
Freeze-dried acellular dermal matrix graft: effects of rehydration on physical, chemical, and mechanical properties
MC Bottino, MV Jose, V Thomas, DR Dean, GM Janowski
dental materials 25 (9), 1109-1115, 2009
782009
The effect of particle size and volume fraction on the aging behavior of a liquid-phase sintered SiC/aluminum composite
GM Janowski, BJ Pletka
Metallurgical and Materials Transactions A 26, 3027-3035, 1995
701995
The microstructure of electrodeposited titanium-aluminum alloys
GM Janowski, GR Stafford
Metallurgical Transactions A 23, 2715-2723, 1992
641992
Design and manufacture of woven reinforced glass/polypropylene composites for mass transit floor structure
UK Vaidya, F Samalot, S Pillay, GM Janowski, G Husman, K Gleich
Journal of Composite Materials 38 (21), 1949-1971, 2004
542004
Microstructural characterization of white layers formed during hard turning and grinding
YB Guo, GM Janowski
Transactions of the North American Manufacturing Research Institute of SME …, 2004
532004
A technique for sputter coating of ceramic reinforcement particles
B Wang, Z Ji, FT Zimone, GM Janowski, JM Rigsbee
Surface and Coatings Technology 91 (1-2), 64-68, 1997
491997